POLYMER CLASS | Polymethacrylate |
COMMON NAMES | Poly(2,2,3,3-tetrafluoropropyl methacrylate) |
STRUCTURE BASED NAME | Poly(2,2,3,3-tetrafluoropropyl 2-methylpropenoate) |
ACRONYMS | |
CAS # | |
CurlySMILES | C{-}C{n+}(C)(C(=O)OCC(F)(F)C(F)F |
CAS # | 45102-52-1 |
COMMON NAMES | 2,2,3,3-Tetrafluoropropyl methacrylate |
SMILES | FC(F)C(F)(F)COC(=O)C(=C)C |
Std. InChI | InChI=1S/C7H8F4O2/c1-4(2)5(12)13-3-7(10,11)6(8)9/h6H,1,3H2,2H3 |
Std. InChIKey | RSVZYSKAPMBSMY-UHFFFAOYSA-N |
STRUCTURE |
![]() |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molar Volume Vm | mL mol-1 | 122.5 | |
Density ρ | g mL-1 | 1.52 | |
Solubility Parameter δ | MPa1/2 | ||
Molar Cohesive Energy Ecoh | J mol-1 | ||
Glass Transition Temperature Tg | K | 339 - 353 | 344 |
Molar Heat Capacity Cp | J (mol K)-1 | ||
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none | 1.417 - 1.422 | 1.42 |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 | 186.1 | |
Van-der-Waals Volume VvW | mL mol-1 | 74.0 | |
Molar Volume Vm | mL mol-1 | 114.8 - 122.5 | 119.3 |
Density ρ | g mL-1 | 1.52 - 1.58 | 1.54 |
Solubility Parameter δ | MPa1/2 | 15.6- 16.7 | 16.2 |
Molar Cohesive Energy Ecoh | J mol-1 | 33600 - 37000 | 35200 |
Glass Transition Temperature Tg | K | 337- 345 | 341 |
Molar Heat Capacity Cp | J (mol K)-1 | 195 - 249 | 233 |
Entanglement Molecular Weight Me | g mol-1 | 25400 - 32800 | 29000 |
Index of Refraction n | none | 1.41 - 1.43 | 1.42 |
Last updated: October 25, 2015